简介:Inthispaper,thebrazingmechanismofLY12aluminumalloyatmiddlerangetemperaturewaspresented.TheCsF-AlF3non-corrosivefluxwasutilizedtoremovethecomplexoxidefilmonthesurfaceofLY12aluminumalloy.TheresultsrevealedthattheoxidefilmwasremovedbytheimprovedCsF-AlF3fluxaccompaniedwiththeoccurrenceofreactionaswellasdissolutionandthecompoundsCsFplayedanimportantroletoremovetheoxidefilm.Actually,thehighactivityofflux,say,theabilitytoremovetheoxidefilm,wasduetothepresenceofthecompounds,suchasNH4F,NH4AlF4andcompositemoltensalt.TheproductionofHFwasthekeyissuetoacceleratethereactionandenhancetoeliminatetheoxidefilmbydissolution.ItwasfoundthattherareearthelementLaatsmallpercentagewasnotenrichedattheinterface.Moreover,therareearthfluorideenhancedthedissolutionbehavior.
简介:ThevacuuminductionbrazingofSiCparticulatereinforcedLY12alloymatrixcompositeusingAl-28Cu-5Si-2Mgfillermetalhasbeencarriedout.Themicrographofthejointinterfacewasobservedbyscanningelectronmicroscopy.Thejointstrengthwasdeterminedbysheartests.Theresultsshowthatbrazingtemperature,holdingtime,SiCparticlevolumepercentageandpostheattreatmentinfluencejointstrength.SiCparticleshappeninthebrazingseamandthedistributionofSiCparticlesinthejointisnotuniform.Particle-poorzonesinthejointexistnearthebasemetal,andparticleconcentratezonesexistinthecenterofthebrazingseam.Inaddition,thefailureofthecompositeispredominantlyinitiatedbytherootingofSiCparticleinthebrazingseamandthemicro-crackexpandedalongthebrazingseamwithlowenergy.
简介:Inthispaperanewmethodforpreventingweldinghotcracking—theinversestrainmethod(ISM)isdevelopedontheprincipleofweldingmechan-ics.EffectivenessandfeasiblityofmethodinpreventingweldinghotcrackingofhighstrengthaluminumalloyLY12CZbysynchronousrollingduringwelding(SRDW)alongbothsidesoftheweldatasuitabledistancebehindtheweldingarcareexamined.ExperimentalresulteindicatethatweldinghotcrackingofLY12CYcanbeeffectivelypreventedandthemechanicalpropertiesofweldedjointcanalsobeimprovedbythemethod.Itisanimportantnewsolutionforpreventinghotcrackinginweldingofsheetmetal.
简介:Themechanicalproperties,creepdamage,creeprupturestrengthandfeaturesofinterfacialfailuresofweldedjointsbetweenmartensite(SA213T91)andpearlitesteel(12Cr1MoV)havebeeninvestigatedbymeansofargontungstenpulsedarcwelding,hightemperatureacceleratedsimulation,creeprupture,mechanicalpropertytestsandscanningelectronicmicroscope(SEM).Theresearchresultsindicatethatthemechanicalpropertiesofovermatchedandmediummatchedjointdeteriorateobviously,andtheyaresusceptibletocreepdamageandfailureafteracceleratedsimulationoperation500h,intheconditionofpreheat250℃,andpostweldingheattreatment750℃×1h.However,themechanicalpropertiesofundermatchedjointarethebest,theinterfacialfailuretendencyofundermatchedweldedjointislessthanthoseofmediumandovermatchedweldedjoint.Therefore,itisreasonablethatlowalloymaterialTR31isusedasthefillermetalofweldbetweenSA213T91and12Cr1MoVsteel.