3-17 Corrosion Studies of MAX Phase in Liquid Pb-Bi Alloy

(整期优先)网络出版时间:2014-01-11
/ 1
Asoneofcandidatesforthefuelcladdingorstructurematerialusedinfourthgenerationfissionandfusiondemonstratereactor,MAXphasehasthepropertiesofbothceramicandmetal,suchashighmeltingpoint,hightemperaturestability,gooderosionresistanceandradiation-damagetolerance[1;2].Maxphaseisaseriesofceramicsofnanolamellarandhexagonalstructure.Mrepresentstransitionelement.Arepresentsthethirdorfourthmaingroupelement.XrepresentNandC.Inthedesignoflead-cooledfastreactor,itisrequiredthatthematerialshouldendurethecorrosionofliquidPb-Bialloy.Therefore,understandingoftheoxidelayersandtheirgrowthmechanismsinLBEisfundamentallyimportantforthedevelopmentofcandidatematerials.